I did some more testing and what works best for me is K1.1, 3.25mm retract, 0 coast
[attachment=1]stringK1.1-3.25mmret-190c.jpg[/attachment]
did some testing on extrude temp and it looks like 195 is the highest I can go before stringing and oozing on the pillars starts. 190 still looks the best to me, the layers look the most defined, no bulging or globbiness. Is there any reason not to print PLA @ 190c?
[attachment=0]stringK1.1-3.25mmret-190-210c.jpg[/attachment]